🏡 Home

Structural Stress Map

Engineering Analysis: Where & Why Jewelry Fails

Engineering Note: Stress concentration factor (Kt) is highest at sharp transitions and solder joints.
VIEW: CROSS_SECTION
MODE: STRESS_ANALYSIS
FAILURE PROBABILITY
High
PRIMARY FORCE
Friction
Loading data...

How to Read This Map

Red Zones (Critical): Areas that experience maximum mechanical stress or material loss. 90% of repairs happen here.

Yellow Zones (Caution): Areas prone to deformation (bending) rather than breaking.

Why 22K/24K Fails Faster: Pure gold has no crystal lattice "memory". Once bent, it stays bent. It wears away 3x faster than 18K due to friction.